Default Stern Drive Anode

I noticed the tiniest bit of oxidation on my boat's stern drive and my neighbor recommended I install an anode (and I've since learned that it ought to be a magnesium anode). I'm not certain what to do or where to install it/what style to get. The sterndrive is Volvo-Penta with an aluminum prop. Thoughts?
upnorth is offline   Reply With Quote
Old 03-25-2008, 01:20 PM   #2
Blue Thunder
Senior Member
 
Blue Thunder's Avatar
 
Join Date: Apr 2004
Location: Eastern MA & Frye Island/Sebago Lake, Maine
Posts: 935
Thanks: 247
Thanked 323 Times in 148 Posts
Default

Quote:
Originally Posted by upnorth View Post
I noticed the tiniest bit of oxidation on my boat's stern drive and my neighbor recommended I install an anode (and I've since learned that it ought to be a magnesium anode). I'm not certain what to do or where to install it/what style to get. The sterndrive is Volvo-Penta with an aluminum prop. Thoughts?
If it's a Volvo it should already have some type of anode on it. The problem is Volvo ships all of their drives, regardless of where they are going with salt water anodes. I, and most of us, I would assume, use our boats in fresh water only or at least most of the time. My Volvo DP drive (2000 Four Winns)pitted significantly before I could research the problem and you're right, you want magnesium not zinc for fresh water.

Blue Thunder
__________________
" Live for today because yesterday is gone and tomorrow may never come"
Blue Thunder is offline   Reply With Quote
Old 03-25-2008, 01:39 PM   #3
codeman671
Senior Member
 
codeman671's Avatar
 
Join Date: Jan 2005
Posts: 3,360
Thanks: 210
Thanked 764 Times in 448 Posts
Default

You are correct on magnesium. Zinc tends to corrode on the outside and scale over instead of dissolving in a uniform manner. Magnesium is a much better choice. I think with the more rapid rate of electrolysis in salt water the zinc does not have time to scale and works just fine.
codeman671 is offline   Reply With Quote
Old 03-25-2008, 01:48 PM   #4
GWC...
Senior Member
 
GWC...'s Avatar
 
Join Date: Apr 2004
Posts: 1,325
Thanks: 5
Thanked 0 Times in 0 Posts
Default

Review the reply that starts, "This is from boatzincs.com"

http://www.boatered.com/forum/topic.asp?TOPIC_ID=112161
__________________
[Assume funny, clever sig is here. Laugh and reflect... ]
GWC... is offline   Reply With Quote
Old 03-25-2008, 02:16 PM   #5
TomC
Senior Member
 
TomC's Avatar
 
Join Date: Apr 2004
Location: Lakes Region
Posts: 547
Thanks: 9
Thanked 29 Times in 20 Posts
Default more than one anode

I have more experience with Mercruisers than VP, but I wanted to point out that you likely have several anodes (4-6) on the outdrive - the discussion here implies there is just one, which is likely not the case.

All of them need to be changed over to magnesium for fresh water use - they each protect different sections of the upper and lower drive assemblies...
TomC is offline   Reply With Quote
Sponsored Links
Old 03-26-2008, 07:02 AM   #6
Phantom
Senior Member
 
Phantom's Avatar
 
Join Date: Jul 2005
Location: Berlin, Ma / Gilford
Posts: 1,931
Thanks: 445
Thanked 604 Times in 340 Posts
Default

Quote:
Originally Posted by upnorth View Post
I'm not certain what to do or where to install it/what style to get. The sterndrive is Volvo-Penta with an aluminum prop. Thoughts?

Perhaps this will help !!

http://www.boatzincs.com/volvo_penta-magnesium.html


And for those of you with MerCruiser -- and wonder where the annodes are ........... This gives a great pictorial

http://www.boatzincs.com/bravo3-mag-kit.html for Bravo 3

http://www.boatzincs.com/alpha-one-gen2-mag-kit.html For Alpha 1
__________________
A bad day on the Big Lake (although I've never had one) - Still beats a day at the office!!
Phantom is offline   Reply With Quote
Old 03-26-2008, 10:20 AM   #7
Grady223
Senior Member
 
Grady223's Avatar
 
Join Date: Apr 2004
Location: New Hope, PA & Barndoor Island
Posts: 464
Thanks: 93
Thanked 24 Times in 18 Posts
Default

Do you need anodes on outboards, too? I have a Merc and a Yamaha. Never noticed if they have them.
Grady223 is offline   Reply With Quote
Old 03-26-2008, 11:50 AM   #8
Dave R
Senior Member
 
Dave R's Avatar
 
Join Date: Jul 2004
Posts: 2,974
Thanks: 246
Thanked 736 Times in 438 Posts
Default

Quote:
Originally Posted by Grady223 View Post
Do you need anodes on outboards, too? I have a Merc and a Yamaha. Never noticed if they have them.

I would fully expect anodes on your lower unit. Any time there's two or more types of metal in the water, the least noble of metals will dissolve through electrolosis. Anodes are less noble than the rest of the lower unit, so they dissolve first. If you tilt the the thing out of the water whenever it's at rest, the anodes will last years in our water.
Dave R is offline   Reply With Quote
Old 03-27-2008, 07:11 AM   #9
Phantom
Senior Member
 
Phantom's Avatar
 
Join Date: Jul 2005
Location: Berlin, Ma / Gilford
Posts: 1,931
Thanks: 445
Thanked 604 Times in 340 Posts
Default

Grady -- I would be SHOCKED if your outboards lower unit did not have them.

On the Merc, look at the under side of the Cavitation plate (above the prop).
__________________
A bad day on the Big Lake (although I've never had one) - Still beats a day at the office!!
Phantom is offline   Reply With Quote
Old 03-27-2008, 08:33 AM   #10
Nauset
Senior Member
 
Nauset's Avatar
 
Join Date: Mar 2007
Posts: 95
Thanks: 2
Thanked 8 Times in 5 Posts
Default

Quote:
Originally Posted by upnorth View Post
I noticed the tiniest bit of oxidation on my boat's stern drive and my neighbor recommended I install an anode (and I've since learned that it ought to be a magnesium anode). I'm not certain what to do or where to install it/what style to get. The sterndrive is Volvo-Penta with an aluminum prop. Thoughts?
What year & model of VP do you have? I have a 2000 DP-S which has two anodes. You should definitely go with mag anodes. Don't waste your time with Boatzincs.com, I tried to get mag anodes from them last year and got the run-around. Go see Charlie at Thurston's Marina Parts Dept. He got them for me in a week.
Nauset is offline   Reply With Quote
Old 05-03-2008, 06:55 PM   #11
jayp603
Senior Member
 
Join Date: Feb 2008
Posts: 50
Thanks: 3
Thanked 5 Times in 2 Posts
Default can u tell by looking?

what type they are? how do i tell if my alpha 1 has salt or fresh water anodes?
jayp603 is offline   Reply With Quote
Old 05-03-2008, 08:23 PM   #12
chunt
Member
 
Join Date: Jan 2005
Posts: 20
Thanks: 0
Thanked 0 Times in 0 Posts
Default

bravo 3 drives use an aluminum anode. The idea being, the bare anode will carode before the painted i/o.
chunt is offline   Reply With Quote
Old 05-04-2008, 09:38 AM   #13
Dave R
Senior Member
 
Dave R's Avatar
 
Join Date: Jul 2004
Posts: 2,974
Thanks: 246
Thanked 736 Times in 438 Posts
Default

Quote:
Originally Posted by chunt View Post
bravo 3 drives use an aluminum anode. The idea being, the bare anode will carode before the painted i/o.
I took the aluminum anodes off mine and put on magnesium.
Dave R is offline   Reply With Quote
Reply

Bookmarks


Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is On
HTML code is On

Forum Jump


All times are GMT -5. The time now is 12:14 AM.


Powered by vBulletin® Version 3.8.11
Copyright ©2000 - 2024, vBulletin Solutions Inc.

This page was generated in 0.28917 seconds